  6. JUDUL                     : THE EFECTIVITY IN ADDING LIMESTONE OF MORTAR FOR PLASTER AND FIXED OF BUILDING :  IN THE CASE STUDY OF MORTAR COMPRESSIVE STRENGTH  TEST
  7. PENELITI                 : APRILLYANI SOFA MARWANINGTYAZ
  8. PEMBIMBING         : MOH RAUF, S.Pd, M.Si
  9. ABSTRAK PENELITIAN

The utilization of  the grind lime stone as the mixed material  for plaster and fixing of  building is rarely used.  Limestone has CaO which is 60% untill 80%, it can be decreased the use of  cement.

Memuat foto

Memuat foto

Memuat foto

This reaserch has function for knowing how strenght-pressure of mortar and  cement mixed by one grind limestone and percentage of grind chalk- stone which has  the  strenght-pressure of mortar standard. Testing instrument of strength-pressure  has cube shaped which has 60 mm x 60 mm x 60 mm. The testing strength pressure of material was tested in Material and Construction laboratory, civil engineering of  Diponegoro University Semarang. It was tasted when the mortal was 8 days made. Mortar has been given the grind limestone based on different content.

It contents  cement : sand :grind chalk-stone 1: 6:2 and 1:7:3. Mortar produced the highest standard of strenght-pressure  than type of N Mortal. In this composition has 1:7:3, mortar can be holded more than 10,56 kg/cm2 and it can decrease using of cement more than 25% without losing the strenght-pressure  of mortar based on Indonesia Standard 15-3758-2504